화학공학소재연구정보센터
검색결과 : 1,520건
No. Article
991 Investigation on strength and corrosion behaviour of friction stir welded similar and dissimilar aluminium alloys
Braun R, Mercado UA, Biallas G
Materials Science Forum, 519-521, 1113, 2006
992 Optimisation of the strength of aluminium foam sandwich (AFS) panels by different heat treatments
Shabestari SG, Wanderka N, Seeliger W, Banhart J
Materials Science Forum, 519-521, 1221, 2006
993 Hardness of oxide scales on Fe-Si alloys at room- and high-temperatures
Amano T, Okazaki M, Takezawa Y, Shiino A, Takeda M, Onishi T, Seto K, Ohkubo A, Shishido T
Materials Science Forum, 522-523, 469, 2006
994 Mechanochemistry: The last energetic frontier
Eckhardt CJ
Molecular Crystals and Liquid Crystals, 456, 1, 2006
995 Analysis of the grinding of toner sheets using Vickers hardness as an index of grindability
Tanaka M, Kamiya H
Powder Technology, 164(2), 82, 2006
996 Phase transformation and hardness of the Ni-P-Al ternary coatings under thermal annealing
Wu FB, Tien SK, Tsai YZ, Duh JG
Thin Solid Films, 494(1-2), 151, 2006
997 Indenter surface area and hardness determination by means of a FEM-supported simulation of nanoindentation
Bouzakis KD, Michailidis N
Thin Solid Films, 494(1-2), 155, 2006
998 Nanoindentation and residual stress measurements of yttria-stablized zirconia composite coatings produced by electrophoretic deposition
Lu X, Wang X, Xiao P
Thin Solid Films, 494(1-2), 223, 2006
999 Microstructure and tribological behaviour of super-hard Ti-Si-C-N nanocomposite coatings deposited by plasma enhanced chemical vapour deposition
Ma DY, Ma SL, Dong HS, Xu KW, Bell T
Thin Solid Films, 496(2), 438, 2006
1000 Fracture toughness, hardness and elastic modulus of hydrogenated amorphous carbon films deposited by chemical vapor deposition
Michel MD, Muhlen LV, Achete CA, Lepienski CM
Thin Solid Films, 496(2), 481, 2006