1 |
사용된 IN738LC 가스 터빈 블레이드 코팅층의 고온 부식 및 Thermally Grown Oxide 형성 거동 최병학, 한성희, 김대현, 안종기, 이재현, 최광수 Korean Journal of Materials Research, 32(4), 200, 2022 |
2 |
Effect of Al-Y gradient coating on hot corrosion resistance of gamma-TiAl alloy at different temperatures Lin H, Liang WP, Jia YL, Miao Q, Hu RY, Ding Z, Yu LJ Applied Surface Science, 487, 868, 2019 |
3 |
Corrosion behavior of Ni-Al alloys beneath chlorides melt salt at 700 degrees C Guo LL, Yue Y, Pan TJ, Tang ZF, Liu W Solar Energy, 184, 657, 2019 |
4 |
Hot corrosion behavior of YSZ, Gd2Zr2O7 and YSZ/Gd2Zr2O7 thermal barrier coatings exposed to molten sulfate and vanadate salt Ozgurluk Y, Doleker KM, Karaoglanli AC Applied Surface Science, 438, 96, 2018 |
5 |
Hot corrosion of Gd2O3-doped CeO2 electrolyte in solid oxide fuel cells with it a liquid antimony anode Ma JY, Duan NQ, Han Y, Yan D, Chi B, Pu J, Li J Journal of Power Sources, 401, 397, 2018 |
6 |
Hot corrosion performance and electrochemical study of CoNiCrAlY/YSZ/YSZ-La2O3 multilayer thermal barrier coatings in the presence of molten salt Khajezadeh MH, Mohammadi M, Ghatee M Materials Chemistry and Physics, 220, 23, 2018 |
7 |
Hot corrosion behavior of commercial alloys in thermal energy storage material of molten MgCl2/KCl/NaCl under inert atmosphere Ding WJ, Shi H, Xiu YL, Bonk A, Weisenburger A, Jianu A, Bauer T Solar Energy Materials and Solar Cells, 184, 22, 2018 |
8 |
Hot corrosion behavior of Ni based Inconel 617 and Inconel 738 superalloys El-Awadi GA, Abdel-Samad S, Elshazly ES Applied Surface Science, 378, 224, 2016 |
9 |
Hot corrosion failure mechanism of graphite materials in molten solar salt Xu YT, Xia TD, Wang WP, Zhang GL, Jia BL Solar Energy Materials and Solar Cells, 132, 260, 2015 |
10 |
Microstructure and hot corrosion behaviors of two Co modified aluminide coatings on a Ni-based superalloy at 700 degrees C Fan QX, Jiang SM, Yu HJ, Gong J, Sun C Applied Surface Science, 311, 214, 2014 |